Product Details:
|
Type: | Round | Application: | Construction,decoration,Industry,Mechineal,shipbuilding |
---|---|---|---|
Standard: | DIN,ASTM,AISI,JIS,EN | Grade: | 17-4PH |
Dimensions: | 5.5mm-500mm | Surface: | Bright,Polished |
Technique: | Cold Rolled Hot Rolled | Length: | Customers' Requirements |
Packing: | Standard Seaworthy Package | Price Term: | CIF CFR FOB Ex-Work |
Highlight: | ss round bars,stainless steel round rod |
Material 17-4ph Stainless Steel Bright Bar Dia 6-30 Mm SUS630 Heat Treated H1150
Alloy 17-4 is a chromium-copper precipitation hardening stainless steel that is used for applications requiring high strength and a moderate level of corrosion resistance. It is one of the most widely used precipitation hardening grades, as it has high strength hardness up to about 572°F while demonstrating good corrosion resistance in all heat treated conditions. Alloy 17-4 has adequate resistance to atmospheric corrosion or in diluted acid salts where its corrosion resistance is equivalent to Alloy 304 or 430. Alloy 17-4 can be heat treated to a variety of temperatures to develop a wide range of properties. Its mechanical properties can be optimized with heat treatment where very high yield strength up to 180 ksi can be achieved. Alloy 17-4 should not be used at temperatures above 572°F or at very low temperatures.
Specifications: UNS S17400
Alloy 17-4 is commonly used for applications requiring high strength and a moderate level of corrosion resistance. Some applications that frequently use Alloy 17-4 include:
TYPE | Cr | Ni | Cu | Cb + Ta | C | Mn | P | S | Si |
---|---|---|---|---|---|---|---|---|---|
17-4 (H900) | min: 15.0 max: 17.5 |
min: 3.0 max: 5.0 |
min: 3.0 max: 5.0 |
min: 0.15 max: 0.45 |
0.07 max |
1.00 max |
0.04 max |
0.03 max |
1.00 max |
Hardening or Precipitation Treatment at 900°F | ||||||
---|---|---|---|---|---|---|
Thickness, inches |
Ultimate Tensile Strength, ksi min. |
0.2% Yield Strength, ksi min. |
Elongation % in 2″ min. | Reduction in Area min. % | Hardness, Rockwell, min. / max |
Hardness, Brinell, min. / max. |
Under 0.1875″ | 190 | 170 | 5 | — | C40 – C48 | — |
0.1875″ to 0.625″ |
190 | 170 | 8 | 25 | C40 – C48 | 388 / 477 |
0.625″ to 4.0″ | 190 | 170 | 10 | 30 | C40 – C48 | 388 / 477 |
Hardening or Aging Treatment at 900°F | ||||||
---|---|---|---|---|---|---|
Thickness, inches |
Ultimate Tensile Strength, ksi min. |
0.2% Yield Strength, ksi min. |
Elongation % in 2″ min. | Reduction in Area min. % | Hardness, Rockwell, min. / max |
Hardness, Brinell, min. / max. |
Up to 3.0 in. incl. | 190 | 170 | 10 | 40 | 40 | 388 |
Over 3.0 in. to 8.0 in. incl. |
190 | 170 | 8 | 35 | 40 | 388 |
Heat Treated Condition | H900 |
---|---|
Density, lbs/in3 | 0.282 |
Electrical Resistivity, microhm-cm | 77 |
Specific Heat, BTU/lb/°F (32-212°F) | 0.10 |
Thermal Conductivity, BTU/hr/ft2/in/°F | |
300°F | 124 |
500°F | 135 |
860°F | 156 |
900°F | 157 |
Mean Coefficient of Thermal Expansion, in/in/°F | |
-100 to 70°F | 5.8 x 10-6 |
70 – 200°F | 6.0 x 10-6 |
70 – 400°F | 6.0 x 10-6 |
70 – 600°F | 6.3 x 10-6 |
70 – 800°F | 6.5 x 10-6 |
70 – 900°F | — |
Modulus of Elasticity, ksi | 28.5 x 103 |
Modulus of Rigidity, ksi | 11.2 x 103 |
Poisson’s Ratio (all conditions) | 0.272 |
Contact Person: Mr. Gao Ben
Tel: +86-18068357371
Fax: 86-0510-88680060