Width: | 600-2500mm | Grade: | S355J2+N |
---|---|---|---|
Technique: | Hot Rolled | Type: | Steel Plate |
Standard: | ASTM,AISI,JIS,DIN | Length: | 1000-12000mm |
Special Use: | High-strength Steel Plate | Thickness: | 6-100mm |
Product Name: | High Quality S355J2+N Hot Rolled Carbon Steel Plate | Shape: | Flat Steel Plate |
High Light: | 10mm Hot Rolled Carbon Steel Plate,1.0577 Hot Rolled Carbon Steel Sheet,S355J2+N Hot Rolled Mild Steel Sheet |
S355J2+N 10*1500*3000mm 1.0577 Steel Plate Hot Rolled Products of Structural Steel EN 10025-2 3.1 Certificate
S355J2 steel (1.0577) is a quality grade of S355 steel, which is one of the non-alloy structural steels commonly used in Europe. According to EN 10025-2: Hot rolled products of structural steels, S355 steel is divided into 4 quality grades, namely:
EN 10025 S355J2 equivalent ASTM A992/A992M; Australian AS/NZS 3678: Grade 350 L20; Canadian G40.20/G40.21: 350WT (55WT); Chinese GB/T 1591: Q355D; and Indian standard IS 2062: E350.
S355J2 Meaning: “S” stands for “Structural steel”; 355 indicates that the material has a minimum yield strength of 355 MPa when the nominal thickness is ≤ 16mm; and “J2” indicates that the material has a minimum impact energy of 27J at -20°C (-4 °F).
S355J2 steel properties are listed in the datasheet below, including chemical composition, physical and mechanical properties, etc.
Chemical composition based on heat analysis.
Chemical Composition, % (≤) | |||||||||
Standard | Steel (Material Number) | C | Si | Mn | P | S | Cu | N | Method of deoxidation |
EN 10025-2 | S355J2 (1.0577) | 0.20 | 0.55 | 1.60 | 0.025 | 0.025 | 0.55 | – | Fully killed |
Note: For carbon content (C) and nominal thickness (t)
Chemical Composition (Product Analysis), % (≤) | |||||||||
Standard | Steel (Material Number) | C | Si | Mn | P | S | Cu | N | Method of deoxidation |
EN 10025-2 | S355J2 (1.0577) | 0.23 | 0.6 | 1.70 | 0.035 | 0.035 | 0.60 | – | Fully killed |
Note: For carbon content (C) and nominal thickness (t)
S355J2 mechanical properties at room temperature are listed in the datasheet below, including tensile strength, yield strength, and elongation, etc.
Yield Strength, Mpa, ≥ | |||||||||
Steel Grade (Steel Number) | t≤16 | 16< t ≤40 | 40< t ≤63 | 63< t ≤80 | 80< t ≤100 | 100< t ≤150 | 150< t ≤200 | 200< t ≤250 | 250< t ≤400 |
S355J2 (1.0577) | 355 | 345 | 335 | 325 | 315 | 295 | 285 | 275 | 265 |
Tensile Strength, Mpa, ≥ | |||
Steel Grade (Material Number) | t<3 | 3 ≤ t ≤ 100 | 100 < t ≤400 |
S355J2 (1.0577) | 510-680 | 470-630 | 450-600 |